Item | Unit | Content |
D10
| μm
| 0.2~0.6
|
D50
| μm
| 0.9~1.8
|
D90
| μm
| ≤10.0
|
Dmax | μm | 34 |
Tap Density
| g/ml
| ≥0.65
|
Specific Surface Area | m2/g | ≤6.0 |
Purity | % | >98 |
Capacity at 0.5C discharging | mAh/g | >161.2 |
Coulomb rate at first cycle | % | 95.5 |
Capacity at 1C discharging
| mAh/g
| >150.0
|
Capacity at 10C discharging | mAh/g | >126.1 |
Capacity at 1C Divided by Capacity at 0.5C | % | 91.0 |
Material Safety Data Sheet | |
Artical | Enhanced performance of sulfone- based electrolytes at lithium ion battey electrodes, including the LiNi0. 5Mn1.5O4 high voltage cathode
|
Application Notes: | Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry. 1. Please keep the powder in vacuum box to avoid moisture. 2. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coatingto ensure max. capacity.
|