Lib-PNCM811 is the precursor powder of NCMOH811 for High Capacity NCM Cathode Powder at your own composition. There are 200 grams in one bottle Note: You must mix the precursor with LiOH. H2O and calcine the mixed powder at 750- 790oC before use
Specification
Package
200g/bottle in a vacuumed bag
Composition
NCMOH811
Configuration
Sphere
Particle size distribution
D10:5.36 μm D50:11 μm D90:18.6 μm
Magnetic substance
102 ppd
Tap Density
≥1.74 g/cm^3
Water Content
wt%<0.5
PH value
~ 8.38
Mian Element
Required Content (mol)
Ratio (Ni:Co: Mn)
Li
0
0
Ni
47.7247
7.994
Co
6.3195
1.059
Mn
5.6562
0.947
Impurity
Required(ppm)
Typical(ppm)
Ca
<300
16
Cu
<50
1
Fe
<100
15
Mg
<300
2
Na
<500
229
Zn
<100
121
SO4
<5000
3000
Note
MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.