Advanced Features | • Maximum temperature: 1650 ºC - • Vacuum or Atmosphere controlled
- • Induction coil traveling distance: Max. 300 mm
- • Applications: melt purification, directional solidification, or single crystal growth for metallic material
|
Power | • Voltage: AC 220 V, Three Phases- • 50/60Hz
- • 15 KW
|
PLC Control | • Touch Screen, User-Friendly- • Parameters: Induction coil and crucible position, Moving speed, Induction power by percentage,
Temperature
|
Working Temperature | • Induction Heating with 15 KW power supply- • Maximum Working Temperature: 1650°C ( <1hr)
- • Frequency: 30 - 80 KHz
|
Tube and Flange | • 2" O.D. High purity quartz tube- • Top stainless steel flange with KF 25 vacuum connection port, mechanical pressure gauge, adjustable
high-pressure relief valve - • Bottom stainless steel flange with the gas delivery port and 1/4" Feedthrough for the thermal couple
- • Graphite crucible 40 mm O.D x 60 mm H with the Boron Nitride Liner
- • One thermal couple on the bottom of the crucible for temperature control
|
Coil Traveling Mechanism | • Maximum traveling distance: 300 mm- • Coil travel range: 150 mm
- • Server motor controlled
- • High speed: 0 - 200 mm/min
- • Slow speed for single crystal growth: 0 - 50 mm/hr
- • The speed mode could be customized with extra cost
|
Water Chiller
| • Temperature range: 5 - 30°C- • Water Flow Rate: 16 L/min
- • Water Tank: 12 Liters made of stainless steel
- • Note: It is recommended to use a specific coolant to get the best performance.
|
Vacuum Pump (Not included) | • 10E-2 torr via dual stage mechanical vacuum pump (bottom right picture)- • 10E-5 torr via Turbopump (bottom left picture)
- • The vacuum pump is optional. Please click here to choose a vacuum pump.
-
|
Compliance | • CE certified- • NRTL certification is available upon request at the extra cost
|
Warranty | - • One Year limited warranty with lifetime support
|
Dimension
| - • 600 mm L X 500 mm W X 800 mm H
|
Net Weight | |
Shipping Weight & Dimensions | |
Installation Video | |
Application note | • In order to zone melting for metallic materials, you may make a solid rod sample from powder before zone melting via CIP as the link below
|