Nanopowder needed to be dispersed before use. Please click here to learnhow to disperse nano powerand click picture below left to order Ultrasonic processor
Please always keep nanopowder in vacuum chamber or glove box to avoid aggregation (click picture below-right to order)
1. It is suggested to use Sodium Alginate as the binder for Si/C Anode 2. You may also consider using our SBR + CMC combination 3. Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry. 4. Please keep the powder in vacuum box to avoid moisture. 5. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.