Model Number | EQ-Die-18D-B |
Pressure Force | 27 ton max. |
Material | Rc 60 - 62 hardened steel Ra 0.08μm highly polished steel All pressing dies are made by high-stretched carbon steel to achieve high hardness to meet the essential requirements of making ceramic or metal samples. Otherwise, the pressing surface could probably get scratched.
|
Dimensions
| B. Sleeve O.D. : ⌀50mm C. Die Sleeve Height: ⌀50mm D. Sleeve I.D. : ⌀19mm + 0.03-0.05mm G. Pressing Rod Diameter: ⌀19mm ± 0.1mm
|
Weight | 2.0 lbs. |
Material Requirement
| • 32-75 Microns- • Do not use this die set for pressing powder with a particle size of 30 micron or smaller; Small particles
may slip into the gap of the die parts and damages the sleeve during the compression. - • Ball mill or ground the powder to the size of 32~75 microns powder before pressing. Please consider
using the 3'' Dia. Sieve Set No.200&450 Mesh to separate the 32~75 microns particles from the powder clumps. - • For pressing sticky metal powders such as Al, Mg, Zn, it is necessary to use dry or alcohol-based tool
lubricant to lubricate the die and sleeve set to reduce friction during the compression.
|
Package Content
| • One pressing die sleeve- • One top pressing die
- • One bottom pressing die
- • One support plate
- • One die kit container
|
Safety Precaution
| • To avoid the risk of accidents and damage to the Pressing Die, please read these instructions carefully before installation and before using it for the first time.- • Read the manual, especially the die installation schematic, before the operation.
- • Do not press flammable, explosive materials.
- • The operator must wear protection goggle.
- • You must have a hydraulic pellet press equipped with the a Protection Cover, please click the pcitures
to the left to order. - • To avoid damaging the die core and sleeve, we strongly recommend to press powder with a professional
laboratory hydraulic press to ensure the evenest pressing interface and uniform pressure force.
|
Pressing Die Installation Schematic / Instruction
| | | - 1. Mixing and grinding chemical powder by agate mortar
or Ball Mill - 2. Calcine mixed the powder in a high temp furnace under
suitable temperature - 3. Crushing and Grinding calcined powder again by mortar
or ball mill - 4. Put calcined powder into the die
- 5. Pressing sample by a pressing machine under suitable
pressure - 6. Take out pellet sample from die
- 7. Sintering the pellet under suitable temperature
|
|
Application Notes
| • Use ethanol to clean the pressing die before and after use every time- • Use anti-rust oil after the operation and store it in a dry place to avoid rusting.
- • You may consider using EQ-BNMR for easy mold release. Please click the picture to order.
-
|