Chemical Composition and XRD
| Li2O-Al2O3-SiO2-P2O5-TiO2
• P2O5 20-60% • TiO2 20-60% • Al2O3 1-15% • SiO2 1-15% • Li2O 1-15% • XRD |
Shapes & Sizes (Please select from Product Options)
| Round: 19mm Dia
| Square: 5mm x 5mm
| Square: 1 Inch x 1 Inch
| Square: 2 Inch x 2 Inch |
Thickness | 150um ( 0.150 mm ) |
Ionic Conductivity
| 1 to 4 ×10^-4 S/cm at 25℃ Room Temperature ~2 x 10^-5 S/cm at -20℃
|
Physical Properties | • Stable in both air and water • Solid electrolyte/ membrane with prevention against dendrite penetration |
Chemical Resistance | The conductivity of Lithium Ions will not be affected much by water and mild acids • RW(P)JOGIS Class 1 Water resistance • RA(p)JOGIS Class 1 Acid resistance |
Mechanical Properties | • 4 Point Bending Strength at 140N/mm2 • Knoop Hardness 590Hk • Specific Gravity 3.05 |
Thermal Properties (Non-Flammable & Stable up to 600℃)
| The coefficient of Thermal Expansion • 30~350℃ Temperature Range: 94 x 10^-7/K • 350~600℃ Temperature Range: 82 x 10^-7/K |
Application Notes
| Assembly of Li-Air Batteries, please click on the picture below for reference.
Please Click HERE to learn more about the properties of our Li-ion conductive ceramic plate
|
Options | Other sizes (e.g. for use in EQ-STC-LI-AIR and STC-ZINCAIR-W Split Test Cells) available upon request, please contact MTI for additional details. |
Relevant Document | Material Safety Data Sheet |
| • Please click picture below to find more equipment for preparing solid-state electrolyte
|